Fred: no worries, bud. There was a rash of them about 1.5 - 2 years ago (maybe six, IIRC).
I figured that you have gotten a bad batch of epoxy or something and I wasn’t able to contact you to see what I should use, so just went with the JB Weld.
Not as pretty as your epoxy, but it’s all hidden in the shroud and all of the repairs have held up so far (both of mine were this way).
Like I said, it was just a few sets and I’ve never heard of another failing (aside from Paul’s, which was due to an accident) , so I didn’t think too much of it.