Thanks jakeru!

Sweating out the mold release agents by baking at 140 degrees F for 20-30 minutes is what Spies Hecker recommends on one of their tech bulletins for new urethane. I built a cardboard enclosure and ducted my salamander heater to it. Monitored it with a digital temp gun and controlled the temp with a vent flap.

About to apply SH recommended urethane primer and their 2 part paint. They don't recommend an adhesion promoter but lots of guys on the net do. Plus, I'd like to find a "wipe down" prep product safe for urethane.

Just curious if there was any experience here.